Customization: | Available |
---|---|
Type: | Rolling Wire |
Material: | Stainless Steel |
Still deciding? Get samples of $ !
Order Sample
|
Shipping Cost: | Contact the supplier about freight and estimated delivery time. |
---|
Payment Methods: |
![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() |
---|---|
Support payments in USD |
Secure payments: | Every payment you make on Made-in-China.com is protected by the platform. |
---|
Refund policy: | Claim a refund if your order doesn't ship, is missing, or arrives with product issues. |
---|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Mechanical properties of the molten metal:
sports event | tensile strength Rm/MPa | yield strength ReL/Rp0.2MPa | elongation A% |
standard value | 490-670 | >=490 | >=18 |
example value | 564 | 459 | 29 |
sports event | C | Mn | Si | S | P | Cr | Ni | Cu |
standard value | <=0.12 | 1.50-1.90 | <=0.07 | <=0.030 | <=0.030 | <=0.20 | <=0.30 | <=0.35 |
example value | 0.11 | 1.65 | 0.05 | 0.017 | 0.022 | 0.022 | 0.02 | 0.116 |
Precautions:
1. The use of flux should be baked at 250-400 ºC for 1-2 hours, welding wire should be dry, oil-free, rust-free state before use.
2. Telding before welding to remove rust, oil and water and other impurities.
3. Sulfur content of the flux <= 0.050% Phosphorus content <= 0.060%.