Customization: | Available |
---|---|
Type: | Rolling Wire |
Material: | Stainless Steel |
Still deciding? Get samples of $ !
Order Sample
|
Shipping Cost: | Contact the supplier about freight and estimated delivery time. |
---|
Payment Methods: |
![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() |
---|---|
Support payments in USD |
Secure payments: | Every payment you make on Made-in-China.com is protected by the platform. |
---|
Refund policy: | Claim a refund if your order doesn't ship, is missing, or arrives with product issues. |
---|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Exemplary Mechanical Attributes of the Molten Metal:
sports event | tensile strength Rm/MPa | yield strength ReL/Rp0.2MPa | elongation A% |
standard value | 490-670 | >=490 | >=18 |
example value | 564 | 459 | 29 |
sports event | C | Mn | Si | S | P | Cr | Ni | Cu |
standard value | <=0.12 | 1.50-1.90 | <=0.07 | <=0.030 | <=0.030 | <=0.20 | <=0.30 | <=0.35 |
example value | 0.11 | 1.65 | 0.05 | 0.017 | 0.022 | 0.022 | 0.02 | 0.116 |
Important Precautions:
1. Ensure the flux is properly baked at temperatures between 250-400 ºC for 1-2 hours. Keep the welding wire in a dry, oil-free, and rust-free condition before commencing use for optimal results.
2. Thoroughly clean the welding area to remove rust, oil, water, and other impurities before starting the welding process.
3. Maintain sulfur content in the flux at <= 0.050% and phosphorus content at <= 0.060% to ensure high-quality welds.